Cyclic olefin copolymer (COC) is chosen when a transparent resin must also be stiff, low-extractable and dimensionally stable — microfluidic chips, diagnostic consumables, optical parts, blister and food packaging. Two names dominate shortlists: TOPAS (Polyplastics) and Mitsui APEL. They are both COC, but the data published on our product pages is organised very differently, and comparing them the wrong way is the most common selection mistake. This guide maps every COC grade currently listed on our site using only the published melt flow rate, density, glass transition temperature (Tg) and Vicat values, so you can shortlist by heat resistance and process before you request a sample.

Contents

The First Trap: MFR Test Temperature Is Not the Same

On the TOPAS pages, melt flow rate is quoted under two different conditions: 230 °C / 2.16 kg and 260 °C / 2.16 kg. This matters more than it looks. A grade measured at 260 °C will show a higher flow number than the same material measured at 230 °C simply because the melt is hotter — so the numbers in the catalogue are not one single comparable scale.

A concrete example from the published data: 5013F-04 is listed at MFR 8 under 230 °C / 2.16 kg, while 5013L-10 and 5013S-04 are listed at MFR 43 under 260 °C / 2.16 kg. It would be wrong to conclude that L-10 and S-04 are "five times more fluid" than F-04 from those two numbers alone — part of that gap is the 30 °C difference in test temperature. Always keep the condition attached to the MFR value, and when two grades sit on different conditions, ask us for a like-for-like figure before you compare.

This is also why the Mitsui APEL grades in our catalogue carry no MFR at all — the published fields on those pages give density and Tg instead. Where a value is not stated in the source data, we leave it blank; we do not estimate it.

The TOPAS Grades (with published MFR)

The table below reproduces the published values on our product pages. MFR is given with its test condition; density is in g/cm³, Tg and Vicat in °C. A dash means the field is not stated — we do not fill it in.

GradeMFR (g/10 min)Test conditionDensityTgVicat
5013F-048230 °C / 2.16 kg1.02133.9—
5013L-1043260 °C / 2.16 kg1.02133.9132.8
5013S-0443260 °C / 2.16 kg1.02133.9132.8
6013F-040.9230 °C / 2.16 kg1.02137.8—
6013M-0712260 °C / 2.16 kg1.02142.2—
6015S-043.6260 °C / 2.16 kg1.02157.8156.1
6017S-041.4260 °C / 2.16 kg1.02177.8177.8
7010F-6009230 °C / 2.16 kg1.02110—
8007F-0410.8230 °C / 2.16 kg1.0177.8—
8007F-60010.8230 °C / 2.16 kg1.0177.8—
8007S-0429260 °C / 2.16 kg1.0177.880
9506F-5005.4230 °C / 2.16 kg1.0163.9—
E-14011260 °C / 2.16 kg0.94—63.9

Two patterns stand out. The 8007 family (8007F-04, 8007F-600, 8007S-04) shares the same Tg of 77.8 °C and density 1.01, but spans three different flow conditions and values — the classic case where the suffix, not the base number, decides process fit. The 6000-series S grades climb sharply in heat resistance: 6013M-07 at Tg 142.2, 6015S-04 at 157.8 and 6017S-04 at 177.8 °C, with flow falling to 3.6 and 1.4 as Tg rises.

The Mitsui APEL Grades (Tg-led)

The APEL pages in our catalogue publish density and glass transition temperature, with no MFR field stated. These values are reproduced exactly as published. Density in g/cm³, Tg in °C.

GradeDensityTg
APL5013VH1.04130
APL5014BH1.05140
APL5014CL1.04135
APL5014DP1.04135
APL5014KL1.04135
APL5014XH1.04140
APL5015AL1.04145
APL5016SL1.04155
APL6011T1.03105
APL6013T1.04125
APL6015T1.04145
APL6509T1.0280

The APEL range reads as a clean heat-resistance ladder. At the low end, APL6509T sits at Tg 80 °C and APL6011T at 105 °C — the choices where the part need not withstand high service temperatures. The APL5014 family clusters tightly at 135–140 °C, which makes the sub-variants (CL, DP, KL, BH, XH) candidates for the same thermal window where other properties or regulatory status will decide. At the top, APL5016SL reaches Tg 155 °C, the highest Tg published in the APEL set.

Selecting by Heat Resistance: Tg Bands

Across both families, the published Tg values fall into three practical bands. Use these as a first cut, then refine by flow and density.

Tg bandTOPAS gradesMitsui APEL gradesTypical fit
Low (≤ 110 °C)9506F-500 (63.9), 8007 family (77.8), 7010F-600 (110)APL6509T (80), APL6011T (105)Packaging, general transparent parts, lower-temperature service
Mid (125–145 °C)5013 family (133.9), 6013F-04 (137.8), 6013M-07 (142.2)APL6013T (125), 5013VH (130), 5014 family (135–140), 5015AL / 6015T (145)Diagnostic consumables, optical parts, general medical devices
High (≥ 155 °C)6015S-04 (157.8), 6017S-04 (177.8)APL5016SL (155)Applications requiring higher heat deflection and sterilisation headroom

Note that Tg is not the same as a sterilisation or heat-deflection rating — it is the temperature at which the polymer transitions from glassy to rubbery. It is the best single number for ranking heat resistance from the data available here, but confirm the specific service condition with the TDS before you specify.

Selecting by Process: Film, Injection and Extrusion

Once heat resistance is fixed, flow decides whether the grade runs on your equipment. Remember the condition caveat above: compare within the same test temperature where possible.

  • High-flow injection moulding — 5013L-10 and 5013S-04 (MFR 43 at 260 °C) suit thin-walled parts and long flow paths. 8007S-04 (MFR 29 at 260 °C) is the high-flow option in the low-Tg band.
  • General-purpose moulding and extrusion — 6013M-07 (12 at 260 °C), 8007F-04 / 8007F-600 (10.8 at 230 °C), 9506F-500 (5.4 at 230 °C) and E-140 (11 at 260 °C) sit in the mid-flow range.
  • Low-flow, high-melt-strength work — 6013F-04 (0.9 at 230 °C), 6017S-04 (1.4 at 260 °C) and 6015S-04 (3.6 at 260 °C) are the slow-flow end, matching the high-Tg end of the range. These are candidates where melt strength matters more than cycle time.
  • Film grades — the F-suffixed 8007F-04 and 8007F-600 share MFR 10.8 and Tg 77.8; consult the TDS for the difference between the two before specifying, since the published fields here are identical.

Density and the E-140 Exception

Nearly every COC grade on these pages sits between 1.01 and 1.05 g/cm³. One grade breaks the pattern: TOPAS E-140 is listed at density 0.94 g/cm³, with a melting point of 83.9 °C and Vicat of 63.9 °C. Its low density and the presence of a melting point rather than a Tg indicate a different structure from the other TOPAS entries. If your selection depends on density or on a specific thermal transition, treat E-140 as a separate case and request its full TDS rather than grouping it with the 8007 or 9506 families.

What to Confirm Before You Place an RFQ

  • Confirm the MFR test condition (230 or 260 °C) for any grade you are comparing — do not compare raw numbers across conditions.
  • State the required Tg or heat-deflection window, and whether the part will see sterilisation temperatures.
  • For APEL grades, request the MFR and flow data separately — those fields are not published on our pages.
  • Ask for the regulatory status you need (food contact, medical, USP Class VI) in writing; it is not stated in the fields reproduced here.
  • Where two grades show identical published values (for example 8007F-04 and 8007F-600), ask what distinguishes them before you choose.
  • Confirm colour, pellet form and packaging, and whether the grade is held in stock or made to order.

FAQ

Can I compare TOPAS MFR at 230 °C directly with MFR at 260 °C?

No. The higher test temperature produces a higher flow reading for the same material. Keep the condition with the number, and ask for a like-for-like measurement when grades are quoted under different conditions.

Why do the Mitsui APEL pages have no MFR?

Because the source data for those grades publishes density and Tg, not melt flow rate. We leave unpublished fields blank rather than estimate them. Ask us for the flow data if it is decisive for your process.

Which COC grade has the highest heat resistance in your catalogue?

By published Tg, TOPAS 6017S-04 at 177.8 °C is the highest, followed by 6015S-04 at 157.8 °C and Mitsui APEL APL5016SL at 155 °C. Confirm the service condition against the TDS before specifying.

Are COC and COP the same material?

They are related but distinct transparent cyclo-olefin resins. We cover the difference separately in COC vs COP: how to choose. This guide is specifically about grade selection within COC.

Do you hold these grades in stock?

Stock varies by grade and region. Send us the grade codes and quantities and we will confirm availability and lead time.