Automotive Weather-Seal Solutions
POE impact modifiers and TPV/TPO routes for lightweight, low-odour door, window and trunk seals.
The buyer's problem
Weather seals — door, window and trunk gaskets — must stay flexible across a wide temperature range, resist UV and ozone, and meet increasingly tight OEM limits on odour and volatile organic compounds (VOC). Traditional EPDM rubber is heavy and hard to recycle. Thermoplastic elastomers (TPE/TPV) and impact-modified polypropylene (TPO) let processors cut part weight, use conventional thermoplastic equipment and regrind scrap, while tuning hardness and compression set to the sealing function. The main selection risk is balancing low-temperature flexibility against heat ageing and fogging performance.
We supply the POE modifier and match it to your compounder's TPO/TPV system; we do not supply finished extruded seal profiles.
How to shortlist the modifier
Low-temperature flexibility
Lower-density, high-comonomer POE keeps the seal soft at low temperature; screen against your OEM cold-flex requirement.
Heat ageing & fogging
Comonomer type and molecular architecture influence compression set and fogging — confirm with your OEM test method.
Processability
MFR is matched to extrusion or injection throughput; too low raises torque, too high can drop melt strength.
Odour / VOC
Confirm the grade meets your OEM's odour and VOC limits with the supplier's current data before tool trials.
POE impact modifiers we can source
POE grades relevant to TPO/TPV weather-seal compounds. Values are transcribed from our on-file TDS; a dash means not on file, to be confirmed with the producer — not a zero.
| Grade | Density g/cm³ | MFR g/10 min | Test condition | Melting °C | Comonomer |
|---|---|---|---|---|---|
| Dow ENGAGE 8150 | — | — | — | — | — |
| ExxonMobil Exact 5371 | — | — | — | — | — |
| Borealis Queo 8210 | 0.882 | 10 | 190 °C / 2.16 kg | 75 | Octene |
| SABIC FORTIFY C13060 | 0.863 | 13 | 190 °C / 2.16 kg | 42 | Octene |
| Wanhua WANSUPER 5136 | 0.865 | 13.5 | 190 °C / 2.16 kg | 59 | ethylene-octene |
| Dow ENGAGE 8400 | 0.87 | 30 | 190 °C / 2.16 kg | 60 | Octene |
Hardness and compression set are tuned in the compound, not set by the base resin alone. Send your OEM spec and we align the modifier shortlist.
Technical reading
FAQ
POE or EPDM for weather seals?
POE-modified TPO/TPV is lighter, processable on thermoplastic equipment and recyclable; EPDM remains established where thermoset performance is specified. The choice depends on your OEM spec and processing route.
Do you supply finished seal profiles?
No. We supply the POE modifier and align it with your compounder's TPO/TPV system. Finished extruded profiles are made by the seal manufacturer.
What does the dash in the table mean?
That TDS field is not on file for the grade. It must be confirmed with the producer before shortlisting — it is not a zero.
Can you meet our OEM odour/VOC limit?
Send the specific OEM method and limit. We will check the grade's current supplier data and flag any gap before you commit to tooling.
Next step
Send your OEM spec — hardness, VOC/fogging limits and processing route — and we propose the modifier package with the matching TDS.
Other application guides on this site: Retort & flexible packaging · Solar encapsulant · Automotive sealing · Wire & cable HFFR · Medical tubing