EVOH Ethylene Content 32 vs 44 mol%: OTR, Processability and Cost

2026-11-12
EVOH Ethylene Content 32 vs 44 mol%: OTR, Processability and Cost

Two numbers dominate almost every EVOH enquiry we receive: 32 and 44 mol% ethylene. One is the high-barrier default for retort and long-shelf-life film; the other is the forgiving, easy-processing grade for coating and deep-draw structures. Buyers often ask which one is "better" — but the honest answer depends on the oxygen transmission rate (OTR) you need, the humidity your package actually sees, and the temperature your line can hold. This article puts the real grade data side by side and shows how to specify the choice. For the full framework, start with our EVOH barrier resin selection guide.

1. Why Ethylene Content Is the First Number to Fix

EVOH is made by saponifying an ethylene-vinyl acetate copolymer. The vinyl alcohol groups form a tight, hydrogen-bonded structure that blocks oxygen extremely well; the ethylene segments bring flexibility, lower moisture uptake and a wider processing window. Every grade is a compromise between the two. More vinyl alcohol means better dry oxygen barrier but higher moisture sensitivity, a higher melting point and a narrower coextrusion window. More ethylene does the opposite.

That is why ethylene content is not a detail you settle after choosing a supplier — it sets the melting point, the MFR you can run, the tie-layer chemistry and the retort behaviour all at once. The EVOH grades on this site are grouped by this number for exactly that reason. If you are still deciding between EVOH, PVDC and nylon, our overview of EVOH grades, ethylene content and OTR covers that comparison first.

2. Real Grade Data: 29 / 32 / 38 / 44 mol%

The table below uses values published on our own grade pages, drawn from manufacturer literature. They are typical values, not specification limits, and the OTR test conditions differ between suppliers — see the note under the table before you compare columns.

Ethylene contentExample grades (linked)Density g/cm³MFR g/10 minTm °CPublished OTR
29 mol%EVASIN EV2951F / Soarnol DT2904RB1.20–1.213.0–3.81880.2–0.3
32 mol%EVASIN EV3251F / Soarnol DC3203RB1.191.6–3.81830.3
38 mol%EVASIN EV3851F / Soarnol E38081.171.6–4.01730.7
44 mol%EVASIN EV4405F / Soarnol A4412B1.144.0–5.5164–1651.5–1.8

OTR figures are quoted as published on the linked pages: Chang Chun EVASIN values are stated for 20 µm film, Nippon Gohsei values at 20 °C / 65% RH. Units and conditions are not identical, so read these as a ranking within a family, not a cross-supplier laboratory comparison. Always confirm the current TDS and its test conditions before ordering.

The trend is consistent across both families: as ethylene content rises from 29 to 44 mol%, density falls from about 1.21 to 1.14 g/cm³, melting point falls from 188 to about 165 °C, and published OTR rises from 0.2–0.3 to 1.5–1.8. A 44 mol% EVAL-type grade shows the same 1.14 g/cm³ / 165 °C pattern. Nothing here is a free lunch — you are trading barrier for processability.

3. What the OTR Numbers Do — and Do Not — Tell You

OTR is measured on a film of a stated thickness at a stated temperature and relative humidity. A number quoted at 20 °C / 65% RH is not comparable to one measured dry, and a number quoted for 20 µm film is not the number your 5 µm layer will deliver. Worse, EVOH is hydrophilic: the hydroxyl groups that give it barrier performance also absorb water. A wet EVOH layer loses a significant part of its oxygen barrier, which is why the resin sits in the core of a multilayer structure rather than on the outside.

Two practical consequences follow. First, a 32 mol% grade only outperforms 44 mol% if the structure keeps the EVOH layer dry enough for that advantage to survive — retort cycles, high-humidity storage and thin polyolefin skins can erase much of it. Second, if your customer's OTR test uses a different humidity from the TDS, the ranking you see on paper may not be the ranking you measure. Ask for OTR at your own conditions, on your own layer thickness, rather than accepting a catalogue number.

4. The Processing Trade: Melting Point, Window and Layer Structure

The melting-point difference in the table is real and operationally important. A 32 mol% grade melting near 183 °C needs a hotter, tighter barrel profile than a 44 mol% grade melting near 165 °C. Lower ethylene content also means a stiffer resin and a narrower window before degradation and gel formation become a concern. Higher ethylene content gives a wider window, better flow and more flexibility — the reason 44 mol% grades are common in coextrusion coating, flexible film and deep-draw sheet.

Decision32 mol%44 mol%
Dry oxygen barrierHigher (published OTR ≈ 0.3)Lower (published OTR 1.5–1.8)
Moisture sensitivityMore pronouncedLess pronounced
Melting point≈ 183 °C≈ 165 °C
Flexibility / deep drawStifferMore flexible
Coextrusion windowNarrower, hotter profileWider, more forgiving
Typical fitHigh-barrier film, retort structuresCoextrusion coating, flexible and deep-draw structures

Both grades still need help from the rest of the structure. EVOH does not bond to polyethylene or polypropylene on its own, so adhesive tie layers sit on either side of the barrier core — see our tie-layer and compatibilizer range. Acid copolymers such as EAA 3330 are also used where adhesion to foil or paper matters. Changing the EVOH grade without re-checking the tie resin and the temperature profile is a common cause of delamination on a new trial.

5. Cost Is a Layer-Thickness Question, Not Just a Resin-Price Question

We do not publish resin prices, and we would be cautious of any comparison that reduces this decision to a per-kilo difference. EVOH is the thinnest layer in the structure — often only a few micrometres — so its share of total material cost is small relative to the polyolefin skins. The levers that actually move cost are how thin you can hold the barrier layer consistently, how much scrap the line makes during start-up, and whether the structure survives the filling or sterilisation cycle first time.

A 32 mol% grade may let you reduce EVOH thickness for a given dry OTR target, but if the narrower processing window increases scrap or forces a slower line, that saving disappears. A 44 mol% grade may need a thicker layer on paper yet run faster and more consistently. Ask for a quote against your actual structure and layer distribution, not against a resin name — and request a sample with a stated lot number for the trial.

6. What to Put in the RFQ

Most costly grade mistakes trace back to an incomplete enquiry. A workable RFQ should state:

  • Target OTR with test temperature, relative humidity and film thickness
  • Full layer order and the intended EVOH layer thickness
  • Filling, hot-fill or retort cycle (time and temperature)
  • Ethylene content and MFR requirement, with the MFR test condition
  • Tie-layer resin on both sides of the barrier core
  • Food-contact compliance required for the destination market
  • Current TDS, SDS and a lot-specific COA for every shipment
  • Sample quantity with lot traceability for the first trial

Our walkthrough of TDS and COA documents explains which six numbers to verify on each lot, and our data sources and TDS request policy sets out how we compile and label the property data on this site. If a figure in a quotation does not appear on the TDS, ask where it came from before you qualify the material.

7. Quick FAQ

Is 32 mol% always the better barrier?

In dry conditions, yes — the published OTR values in the table above rise steadily as ethylene content increases. Under high humidity or after retort, the ranking can narrow or change, because moisture uptake affects the lower-ethylene grades more strongly. Measure at your own conditions.

Can I swap 44 mol% for 32 mol% without re-qualification?

No. Melting point, MFR, stiffness and adhesion behaviour all change, so the barrel profile, tie resin and layer distribution need a fresh trial. Treat it as a new structure, not a like-for-like substitution.

Do I need a tie layer with either grade?

For PE or PP skins, yes. EVOH has poor adhesion to polyolefins on its own; the tie layers are half of the barrier decision. Our selection guide covers layer order in more detail.

Send us your structure, shelf-life target, OTR test conditions and filling cycle, and we will come back with grade options, sample availability and the current TDS for each. Browse the EVOH range or contact the technical team directly.

About This Article

This guide is prepared by the POLYVALA technical team. All property values, test methods and compliance statements are drawn from manufacturer Technical Data Sheets (TDS) and recognized standards (ASTM, ISO). Figures must always be confirmed against the current official TDS and the lot-specific Certificate of Analysis (COA) before production qualification.

References

  • Manufacturer Technical Data Sheets (TDS) for the grades referenced above.
  • ASTM D1238 / ISO 1133 — Melt flow rate (MFR/MFR) of thermoplastics.
  • ASTM D1505 / ISO 1183 — Density of plastics by the density-gradient technique.
  • ASTM D638 — Tensile properties of plastics.

About this article

Written by the technical team at Shanghai Polyvala Plastics, a sourcing and compounding partner for specialty polymer buyers since 2013. We check grades against manufacturer TDS and lot-specific COA rather than marketing claims. Questions about a grade or an equivalent? Request the TDS and COA, or contact our application engineers for a line-specific recommendation.